Huntsman Araldite GZ 488 V-32 US Bisphenol A Epoxy Solution

Category Polymer , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name Araldite
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman Araldite GZ 488 V-32 US Bisphenol A Epoxy Solution.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Weight per Epoxide (EEW, g/eq) 3570 to 5500. Max color is 3.Comments/Applications: Very high molecular weight solid epoxy (8,000 - 10,000), 35% solids in PM acetate. Outstanding adhesion, excellent flexibility and toughness. For use in heat cured industrial coatings with urea, melamine and/or phenolic resins. Viscosity, Gardner Holdt at 25°C: Y-Z2Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 1300 - 3500 cP
1300 - 3500 cP