Material Notes:
Comments/Applications: Max color is 8. Prepolymer of B-10. Used primarily in the manufacture of prepreg for structural composites and tooling. High temperature adhesives.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 250 - 600 cP
250 - 600 cP