Material Notes:
Approx. H+ equivalent weight 115. Mix Ratio with GY 6010 is 60.Comments/Applications: Euredur 43 S is the accelerated version of Euredur 43.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 550 - 850 cP
550 - 850 cP
Processing Properties Metric English Comments
Pot Life 24 min
24 min