Material Notes:
Approx. H+ equivalent weight 77. Mix Ratio with GY 6010 is 30.Comments/Applications: High solids coatings, floorings and tank linings. Good acetic acid resistance and other aggressive environments.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity Measurement <= 100
<= 100
Processing Properties Metric English Comments
Processing Temperature 25.0 °C
77.0 °F
Cure Schedule: 7 days @ 25°C