Indium Corp. 1081 Wave Solder Flux, Water-Soluble

Category Fluid
Manufacturer Indium Corporation of America
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. 1081 Wave Solder Flux, Water-Soluble.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Wave Solder Flux 1081 is a water wash organic solder flux suitable for all conventional tin/lead alloys. 1081 exhibits excellent solderability with low ionic residues after aqueous cleaning.FeaturesExcellent solderabilityWide process windowCleans to low ionic levelsPhysical Properties Color: Light AmberFlux Type Classification: ORH0Information provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Specific Gravity 0.957 g/cc

@Temperature 25.0 °C
0.957 g/cc

@Temperature 77.0 °F
0.963 g/cc

@Temperature 15.5 °C
0.963 g/cc

@Temperature 59.9 °F
Solids Content 28.44 %
28.44 %
Thermal Properties Metric English Comments
Flash Point 18.3 °C
65.0 °F
TCC