Material Notes:
Wave Solder Flux 1085 is a water-soluble flux specifically developed for soldering surface-mount, mixed-technology and through-hole electronic assemblies.1085 is biodegradable and cleans readily in water to low ionic levels, while leaving a surface which has a high surface insulation resistance.FeaturesHigh activity levelLow SolidsCleans to low ionic levelsPhysical Properties Color: PaleFlux Type Classification: ORH0Information provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Specific Gravity 0.860 g/cc

@Temperature 25.0 °C
0.860 g/cc

@Temperature 77.0 °F
0.866 g/cc

@Temperature 15.5 °C
0.866 g/cc

@Temperature 59.9 °F
Solids Content 12.36 %
12.36 %
Thermal Properties Metric English Comments
Flash Point 20.0 °C
68.0 °F
TCC