Material Notes:
Synonyms: Gallium Chloride, Gallium (III) ChlorideCAS Number: 13450-90-3EC Number: 236-610-0RTECS: LW9100000Purity: 99.5 to 99.999% Gallium TrichlorideAppearance: Clear or White, Needle-shaped Crystals; Deliquescent; Fumes in AirForm: Solid Polycrystalline or Free-Flowing GranuleSolubility: Soluble in Water, Ammonia, Benzene, Ethers, Carbon Disulfide, Carbon Tetrachloride.Information provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Density 2.47 g/cc
0.0892 lb/in³
Solid
2.05 g/cc

@Temperature 77.9 °C
0.0741 lb/in³

@Temperature 172 °F
Liquid at mp
Molecular Weight 176.08 g/mol
176.08 g/mol
Vapor Pressure 0.00133 bar

@Temperature 48.0 °C
1.00 torr

@Temperature 118 °F
0.0133 bar

@Temperature 78.0 °C
10.0 torr

@Temperature 172 °F
Thermal Properties Metric English Comments
Melting Point 77.9 °C
172 °F
Boiling Point 201.3 °C

@Pressure 0.101 MPa
394.3 °F

@Pressure 14.7 psi
Component Elements Properties Metric English Comments
Aluminum, Al <= 0.00010 %
<= 0.00010 %
Typical
<= 0.00050 %
<= 0.00050 %
Copper, Cu <= 0.00010 %
<= 0.00010 %
Typical
<= 0.00030 %
<= 0.00030 %
Gallium, Ga 0.39596 %
0.39596 %
Theoretical
Germanium, Ge 0.00010 %
0.00010 %
Typical
0.00050 %
0.00050 %
Indium, In <= 0.00010 %
<= 0.00010 %
Typical
<= 0.00050 %
<= 0.00050 %
Iron, Fe <= 0.00010 %
<= 0.00010 %
Typical
<= 0.00040 %
<= 0.00040 %
Lead, Pb <= 0.00010 %
<= 0.00010 %
Typical
<= 0.00050 %
<= 0.00050 %
Nickel, Ni <= 0.00010 %
<= 0.00010 %
Sodium, Na <= 0.00010 %
<= 0.00010 %
Typical
<= 0.00050 %
<= 0.00050 %
Tin, Sn <= 0.00010 %
<= 0.00010 %
Typical
<= 0.00050 %
<= 0.00050 %
Trace Metals <= 0.00030 %
<= 0.00030 %
Total combined metals, typical
<= 0.0010 %
<= 0.0010 %
Total combined metals
Zinc, Zn <= 0.00010 %
<= 0.00010 %
Typical
<= 0.00050 %
<= 0.00050 %