Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Indorama Auriga Polymers Invistaâ„¢ Polyclearâ„¢ Crystalâ„¢ 3302 PET Resin

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer Indorama Auriga Polymers
Trade Name Invista™ Polyclear™ Crystal™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indorama Auriga Polymers Invistaâ„¢ Polyclearâ„¢ Crystalâ„¢ 3302 PET Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polyclearâ„¢ Crystalâ„¢ PET 3302 is a copolymer packaging resin with a nominal intrinsic viscosity of 0.79 dl/g. Polyclearâ„¢ Crystalâ„¢ PET 3302 is designed to have slow re-crystallization rates, and containers produced from the resin are noted for their excellent color and clarity. Polyclearâ„¢ Crystalâ„¢ PET 3302 has been used successfully in pharmaceutical, personal care, household goods, liquor, and food containers as well as other custom containers. This polymer complies with the Federal Food, Drug, and Cosmetic Act for certain food applications. Please contact INVISTA for specific FDA clearances. Polyclearâ„¢ Crystalâ„¢ PET 3302 offers excellent performance in single-stage, integrated injection-stretch blow molding machines as well as in two-stage, one-step injection and stretch-blow machines. Containers made from INVISTA PET are lightweight, have excellent clarity, and are shatterproof. With the important advantage of being totally recyclable, PET is the packaging material of choice.
Physical Properties Metric English Comments
Bulk Density >= 0.833 g/cc
>= 0.0301 lb/in³
Density >= 1.39 g/cc
>= 0.0502 lb/in³
Pycnometer
Particle Mesh Size 28 Mesh
28 Mesh
0.05% through; Gravimetric determination as manufactured
Viscosity Measurement 0.77 - 0.81
0.77 - 0.81
Intrinsic; WI No. 104
Crystallinity >= 50 %
>= 50 %
Pycnometer
Thermal Properties Metric English Comments
Melting Point <= 248 °C
<= 478 °F
DSC
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Chemical Properties Metric English Comments
Acetaldehyde <= 2.00 ppm
<= 2.00 ppm
Gas Chromatography
Diethylene Glycol <= 2.3 %
<= 2.3 %
Gas Chromatography
Carboxyl End Groups <= 35 meq/kg
<= 35 meq/kg
Titration
Processing Properties Metric English Comments
Moisture Content <= 0.10 %
<= 0.10 %
Karl Fisher Titration as manufactured
Descriptive Properties Value Comments
Chip Size < 2 grams/100 chips
Process Blow Molding
Injection Molding
Region US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved