Indorama Auriga Polymers Polyclearâ„¢ Refresh 1101 PET Resin

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer Indorama Auriga Polymers
Trade Name Polyclear™ Refresh
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indorama Auriga Polymers Polyclearâ„¢ Refresh 1101 PET Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polyclear® Refresh PET 1101 is a copolymer packaging resin with a nominal intrinsic viscosity of 0.83 dl/g. Packaging made from Polyclear® Refresh PET 1101 has excellent clarity and is noted for its dimensional stability, which prevents shrinkage and expansion of the container. Polyclear® Refresh PET 1101 is used successfully in carbonated soft drink bottles and other applications such as water bottles, food containers, and packaging for household goods. This polymer complies with the Federal Food, Drug, and Cosmetic Act for certain food contact applications. Please contact Auriga Polymers Inc. for specific FDA clearances. Polyclear® Refresh PET 1101 offers excellent performance in maximum throughput, stretch blow molding applications. Preforms made from Polyclear® Refresh PET 1101 allow maximum blowing throughputs by quickly heating in the infrared (IR) ovens. In addition, bottles made from Polyclear® Refresh PET 1101 are low-stick, which eases handling issues. Containers made from Auriga Polymers Inc. PET are lightweight, have excellent clarity, and are shatterproof. With the important advantage of being totally recyclable, PET is the packaging material of choice.
Physical Properties Metric English Comments
Bulk Density >= 0.833 g/cc
>= 0.0301 lb/in³
Density >= 1.39 g/cc
>= 0.0502 lb/in³
Pycnometer
Particle Mesh Size 28 Mesh
28 Mesh
0.05% through; Gravimetric determination as manufactured
Viscosity Measurement 0.81 - 0.85
0.81 - 0.85
Intrinsic; 1% Solution in Dichloroacetic Acid
Crystallinity >= 50 %
>= 50 %
Pycnometer
Thermal Properties Metric English Comments
Melting Point <= 252 °C
<= 486 °F
DSC
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Chemical Properties Metric English Comments
Acetaldehyde <= 2.00 ppm
<= 2.00 ppm
Gas Chromatography
Diethylene Glycol <= 1.8 %
<= 1.8 %
Gas Chromatography
Carboxyl End Groups <= 45 meq/kg
<= 45 meq/kg
Titration
Processing Properties Metric English Comments
Moisture Content <= 0.10 %
<= 0.10 %
Karl Fisher Titration as manufactured
Descriptive Properties Value Comments
Chip Size < 2 grams/100 chips
Process Blow Molding
Injection Molding
Region US & Canada
Bamberger Polymers Distribution