Ineos H03SLME Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos H03SLME Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This is a homopolymer designed for extrusion, and it is compliant with both the FDA status and the EU Food Contact status.Information provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Melt Flow 2.5 - 4.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.5 - 4.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238-04