Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos H11G-00 Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Fiber Grade
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos H11G-00 Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This is a barefoot homopolymer designed for fiber applications.ApplicationsStaple FiberOriented YarnBenefitsConsistent processabilityInformation provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Melt Flow 11 g/10 min

@Load 2.16 kg,
Temperature 230 °C
11 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 37.8 MPa

@Temperature 23.0 °C
5480 psi

@Temperature 73.4 °F
Molded and tested under D410, 50 mm/min; ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Modulus 1.68 GPa

@Temperature 23.0 °C
243 ksi

@Temperature 73.4 °F
ASTM D790A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.3 °C
200 °F
ASTM D648
Users viewing this material also viewed the following: