Ineos Nova T263B Expandable Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer Ineos Nova
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos Nova T263B Expandable Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for low density foam.Applications: This grade is used mainly for producing low density block, which are subsequently cut to board insulation.Information provided by NOVA Chemicals.
Physical Properties Metric English Comments
Bulk Density 0.620 g/cc
0.0224 lb/in³
Density 0.00900 - 0.0150 g/cc
0.000325 - 0.000542 lb/in³
Normal molded density assuming cost optimized selection of processing conditions.
>= 0.0120 g/cc
>= 0.000434 lb/in³
Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure
Bead Size 1.18 - 2.36 mm
0.0465 - 0.0929 in
> 95% in this range per Berre Laboratory Analytical Methods 0492
1.30 - 2.40 mm
0.0512 - 0.0945 in
Chemical Properties Metric English Comments
Styrene Content <= 0.10 %
<= 0.10 %
Residual Styrene Monomer Content per Berre Laboratory Analytical Methods 0075
Blowing Agent Content >= 6.2 %
>= 6.2 %