Material Notes:
A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for medium density foam.Applications: This grade is used mainly for producing medium density block which is cut to make board and contour moldings with a wall thickness greater than 10 mm.Information provided by NOVA Chemicals.
Physical Properties Metric English Comments
Bulk Density 0.620 g/cc
0.0224 lb/in³
Density >= 0.0150 g/cc
>= 0.000542 lb/in³
Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure
0.0150 - 0.0300 g/cc
0.000542 - 0.00108 lb/in³
Normal molded density assuming cost optimized selection of processing conditions.
Bead Size 0.500 - 1.00 mm
0.0197 - 0.0394 in
> 95% in this range per Berre Laboratory Analytical Methods 0492
0.700 - 1.00 mm
0.0276 - 0.0394 in
Chemical Properties Metric English Comments
Styrene Content <= 0.10 %
<= 0.10 %
Residual Styrene Monomer Content per Berre Laboratory Analytical Methods 0075
Blowing Agent Content >= 6.0 %
>= 6.0 %