Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Inno-Comp INNOPOL® CS 3-9230 KAR YU UV-Stabilized, 26% Mineral-Filled Compound Blend Of Polypropylene Homopolymer And Block-Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced
Manufacturer Inno-Comp Ltd
Trade Name INNOPOL® CS
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Inno-Comp INNOPOL® CS 3-9230 KAR YU UV-Stabilized, 26% Mineral-Filled Compound Blend Of Polypropylene Homopolymer And Block-Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
INNOPOL® CS 3-9230 KAR YU is a yellow colored, UV-stabilized, 26% mineral-filled compound based on a blend of polypropylene homopolymer and block-copolymer.INNOPOL® CS 3-9230 KAR YU is developed for producing injection molded components for household appliances.All information provided by INNO-COMP.
Physical Properties Metric English Comments
Density 1.12 g/cc

@Temperature 23.0 °C
0.0405 lb/in³

@Temperature 73.4 °F
ISO 1183
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.0 MPa
3770 psi
50 mm/min; ISO 527-1,-2
Elongation at Yield 5.0 %
5.0 %
50 mm/min; ISO 527-1,-2
Tensile Modulus 1.95 GPa
283 ksi
1 mm/min; ISO 527-1,-2
Flexural Modulus 2.05 GPa
297 ksi
2 mm/min; ISO 178
Charpy Impact Unnotched 1.30 J/cm²

@Temperature -20.0 °C
6.19 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eU
5.50 J/cm²

@Temperature 23.0 °C
26.2 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.200 J/cm²

@Temperature -20.0 °C
0.952 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
0.400 J/cm²

@Temperature 23.0 °C
1.90 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 113 °C
235 °F
ISO 75-1,-2
Descriptive Properties Value Comments
Color Yellow
Users viewing this material also viewed the following: