Intercontinental Polymers 131 PET Polymer Type - Semi-Dull, Flame Retardant, Polyester Pellets

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer Intercontinental Polymers, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Intercontinental Polymers 131 PET Polymer Type - Semi-Dull, Flame Retardant, Polyester Pellets.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Filament SpecialtiesInformation provided by Intercontinental Polymers.
Physical Properties Metric English Comments
Viscosity Measurement 0.635 - 0.664
0.635 - 0.664
Intrinsic; LCL-PR21
Optical Properties Metric English Comments
Gardner Color Number 2.0 - 5.0
2.0 - 5.0
+ b; LCL-PR01
61 - 71
61 - 71
Rd; LCL-PR01
Processing Properties Metric English Comments
Melt Temperature 251 °C
484 °F
LCL-PR29
Moisture Content <= 0.40 %
<= 0.40 %
LCL-PR08
Descriptive Properties Value Comments
COOH Max 45 meq/kg
LCL-PR09
DEG 0.7 - 1 wt%
LCL-PR11
Phosphorous 2900 - 3300 ppm
TiO2 0.33 - 0.37 wt%
LCL-PR02