Invista Polyclear® Conserve™ 1101D PET Copolymer Packaging Resin  (discontinued **)

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Invista Polyclear® Conserve™ 1101D PET Copolymer Packaging Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyclear® Conserve™ PET 1101D is a copolymer packaging resin containing 20% post consumer recycled PET. It has a nominal intrinsic viscosity of 0.83 dl/g. Packaging made from Polyclear® Conserve™ PET 1101D has excellent clarity and is noted for its dimensional stability, which prevents shrinkage and expansion of the container. Polyclear® Conserve™ PET 1101D is formulated to be used in carbonated soft drink bottles and other applications such as packaging for food and for household goods. This polymer complies with the Federal Food, Drug, and Cosmetic Act for certain food contact applications. Please contact INVISTA for specific FDA clearances. Polyclear® Conserve™ PET 1101D offers excellent performance in maximum throughput, stretch-blow molding applications. Preforms made from Polyclear® Conserve™ PET 1101D allow maximum blowing throughputs by quickly heating in the infrared (IR) ovens. In addition, bottles made from Polyclear® Conserve™ PET 1101D are low-stick, which eases handling issues. Containers made from INVISTA PET are lightweight, have excellent clarity, and are shatterproof. With the important advantage of being totally recyclable, PET is becoming the packaging material of choice.Carboxyl end groups:
Physical Properties Metric English Comments
Bulk Density >= 0.833 g/cc
>= 0.0301 lb/in³
Packed
Density >= 1.39 g/cc
>= 0.0502 lb/in³
Viscosity Measurement 0.81 - 0.85
0.81 - 0.85
Intrinsic viscosity; WI No. 104 test; correlated from solution viscosity by Invista
Thermal Properties Metric English Comments
Melting Point <= 252 °C
<= 486 °F
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Descriptive Properties Value Comments
Process Blow Molding
Injection Molding