Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Isoflon PTFE + 40% Bronze Polytetrafluoroethylene with 40% Bronze

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Bronze Filled
Manufacturer Isoflon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Isoflon PTFE + 40% Bronze Polytetrafluoroethylene with 40% Bronze.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Properties:Excellent wear and compression resistance (low cold creep)Good thermal conductivityImproved coefficient of friction when combined with Mos² or graphiteApplications: Dynamic seals for wear resistance under high pressure, but when resistance to chemical corrosion is not a necessity.Information provided by Isoflon.
Physical Properties Metric English Comments
Specific Gravity 3.09 - 3.14 g/cc
3.09 - 3.14 g/cc
ASTM D792
Deformation 4.0 - 5.0 %

@Time 86400 sec
4.0 - 5.0 %

@Time 24.0 hour
Permanent, after Relaxation; ASTM D695
7.0 - 10 %

@Pressure 0.0000140 MPa,
Time 86400 sec
7.0 - 10 %

@Pressure 0.00203 psi,
Time 24.0 hour
Under Load; ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 65 - 70
65 - 70
ASTM D2240
Tensile Strength 20.0 - 25.0 MPa
2900 - 3630 psi
ASTM D4894
Elongation at Break 250 - 300 %
250 - 300 %
ASTM D4894
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -200 °C
-328 °F
Copyright © lookpolymers.com All Rights Reserved