Isoflon PTFE + 60% Bronze Polytetrafluoroethylene with 60% Bronze

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Bronze Filled
Manufacturer Isoflon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Isoflon PTFE + 60% Bronze Polytetrafluoroethylene with 60% Bronze.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Properties:Excellent wear and compression resistance (low cold creep)Good thermal conductivityImproved coefficient of friction when combined with Mos² or graphiteApplications: Dynamic seals for wear resistance under high pressure, but when resistance to chemical corrosion is not a necessity.Information provided by Isoflon.
Physical Properties Metric English Comments
Specific Gravity 3.90 - 3.98 g/cc
3.90 - 3.98 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 65 - 70
65 - 70
ASTM D2240
Tensile Strength 17.0 - 22.0 MPa
2470 - 3190 psi
ASTM D4894
Elongation at Break 180 - 220 %
180 - 220 %
ASTM D4894
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -200 °C
-328 °F