KKPC KOSYN KSL 611 Styrene-Butadiene Latex

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Korea Kumho Petrochemical Co., Ltd.
Trade Name KOSYN
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KKPC KOSYN KSL 611 Styrene-Butadiene Latex.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Styrene-Butadiene LatexCharacteristics: High adhesive strength,  excellent printing aptitude, excellent adhesive degree, heat resistance, good dispersion, foam stability, aging resistance, good abrasion resistance, chemical resistance, excellent shock resistance, excellent dispersibility and runnability.Applications: Substitution for Natural LatexThis product is so sensitive to sunlight and humidity that it can be tarnished and caused deterioration of quality if exposed. It is recommended to store it in cool and shady area lest it should be exposed to direct sunlight. Do not expose to incompatible materials or contaminants.Data provided by Korea Kumho Petrochemical Co., Ltd.
Physical Properties Metric English Comments
Solids Content 35 %
35 %
pH 11
11
at 25°C
Viscosity 80 cP
80 cP