Material Notes:
Solution Styrene Butadiene Rubber (S-SBR)Characteristics: This product is made by solution polymerization under which styrene and butadiene react in organic solvent using alkyl-lithium catalyst. It is superior to SBR, which is made by emulsion polymerization, in processability, visco-elasticity and low temperature properties. Also, the products' properties can be adjusted to the purpose of consumption according to the proper proportion of styrene content, the micro structure and the molecular weight.Applications: Shoes, Soles, Tires, Machine Parts, Energy-saving Tires, High-efficiency TiresAdditional Notes: Bound Styrene: 5%cis-1,4 Contents: 7.5%trans-1,4 Contents: 12.5%Vinyl Contents: 80%Dynamic Test: GABO Qualimeter (11Hz)(TAN) 0°C: 0.61210°C: 0.38460°C: 0.10370°C: 0.1This product is so sensitive to sunlight and humidity that it can be tarnished and caused deterioration of quality if exposed. It is recommended to store it in cool and shady area lest it should be exposed to direct sunlight. Do not expose to incompatible materials or contaminants.Data provided by Korea Kumho Petrochemical Co., Ltd.
Physical Properties Metric English Comments
Mooney Viscosity 65

@Temperature 100 °C
65

@Temperature 212 °F
Raw; ML1+4
95.6

@Temperature 100 °C
95.6

@Temperature 212 °F
ML1+4; Polymer 100, HAF Black (IRB#6) 50, ZnO 3, Stearic Acid 1, D 0.3, DM 0.6, Sulfur 1.75, Total: 156.65, Cure: 145°C, 35 minutes.
Mechanical Properties Metric English Comments
Hardness, Shore A 63
63
JIS-A
Tensile Strength, Ultimate 22.8 MPa
3300 psi
Elongation at Break 440 %
440 %
300% Modulus 0.0132 GPa
1.92 ksi
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -17.0 °C
1.40 °F