Karina 1100/2350-IE MBPP White Color Concentrate

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina 1100/2350-IE MBPP White Color Concentrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Filled white color concentrate with CACO3 recommended for extrusion process. Estimated dosage of 2%.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Moisture Absorption <= 0.100 %
<= 0.100 %
ME-52
Ash 71 - 75 %
71 - 75 %
CaCO<sub>3</sub>, ME 51
Descriptive Properties Value Comments
Application Extrusion
Dispersion OK
ME 56
Granulomety 20 - 30
grains/g; ME 05
Recommended Application (%) 2