Karina 75/202 Clear PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina 75/202 Clear PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.23 - 1.27 g/cc
1.23 - 1.27 g/cc
ASTM D 792
Mechanical Properties Metric English Comments
Hardness, Shore A 73 - 77

@Time 15.0 sec
73 - 77

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 8.83 MPa
>= 1280 psi
ASTM D 638
Elongation at Break >= 200 %
>= 200 %
ASTM D 638
Tear Strength >= 40.0 kN/m
>= 228 pli
DIN 53507
Abrasion <= 150
<= 150
mm<sup>3</sup>; DIN 53516
Descriptive Properties Value Comments
Application Sandals
Clarity 0.00 OK
ME 03