Karina E 1000/HMB 21586 White Concentrate Color Concentrate

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 1000/HMB 21586 White Concentrate Color Concentrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Filled white concentrate designed for general purpose film applications based on olefin resins. Letdown ratio estimated from 1% to 5%.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 2.14 - 2.20 g/cc
2.14 - 2.20 g/cc
ASTM D 792
Moisture Absorption <= 0.100 %
<= 0.100 %
ME-52
Ash 83 - 87 %
83 - 87 %
CaCO<sub>3</sub>, ME 51
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 300 °C
572 °F
Heat Resistance; DIN 53772
Descriptive Properties Value Comments
Application Extrusion
Dispersion OK
ME 56
Granulomety 20 - 30
grains/g; ME 05
Lightfastness 8
Scale: 1 to 8
Migration Resistance 5
Scale: 1 to 5
Pellet Form OK