Karina E 18/548-RG-GE Gray Color Concentrate for PVC

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 18/548-RG-GE Gray Color Concentrate for PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Color concentrate recommended for application in rigid PVC compounds for general purposes. Important Considerations:Heavy metal freeFormulated with organic and inorganic pigments PVC resin based (carrier polymer) Supplied in pellet form and packaged in 25 KG bags Recommended use of 2% to 4%Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.23 - 1.29 g/cc
1.23 - 1.29 g/cc
ASTM D 792
ASTM Color -3.55 - -1.55
-3.55 - -1.55
Color B, ME 12
-3.28 - -1.28
-3.28 - -1.28
Color A, ME 12
64.93 - 66.93
64.93 - 66.93
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
ASTM D 2240
Descriptive Properties Value Comments
Application Extrusion
Injection
RAL Classification (Natural Base) 7001