Karina E 20/12-GEN Cream MBATCH (SP31451) for PVC

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 20/12-GEN Cream MBATCH (SP31451) for PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Recommended usage from 2% to 3% on crystal PVC compoundInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
ASTM Color 13.45 - 15.45
13.45 - 15.45
Color A, ME 12
27.68 - 29.68
27.68 - 29.68
Color B, ME 12
68.46 - 70.46
68.46 - 70.46
Color L, ME 12
Descriptive Properties Value Comments
Application Extrusion