Karina E 680D35/1-B-IS Ivory PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 680D35/1-B-IS Ivory PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.24 - 1.30 g/cc
1.24 - 1.30 g/cc
ASTM D 792
ASTM Color -1.65 - 0.35
-1.65 - 0.35
Color A, ME 12
0.48 - 2.48
0.48 - 2.48
Color B, ME 12
88.19 - 90.19
88.19 - 90.19
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 66 - 70

@Time 15.0 sec
66 - 70

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 9.81 MPa
>= 1420 psi
ASTM D 638
Elongation at Break >= 275 %
>= 275 %
ASTM D 638
Descriptive Properties Value Comments
Application General Purpose Profiles