Karina E 836-10/185-ERYB White PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 836-10/185-ERYB White PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.42 - 1.48 g/cc
1.42 - 1.48 g/cc
ASTM D 792
ASTM Color -1.36 - 0.24
-1.36 - 0.24
Color A, ME 12
1.56 - 3.16
1.56 - 3.16
Color B, ME 12
95.64 - 97.24
95.64 - 97.24
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore D 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 38.6 MPa
>= 5600 psi
ASTM D 638
Izod Impact, Notched >= 0.448 J/cm
>= 0.840 ft-lb/in
Method A; ASTM D 256
Thermal Properties Metric English Comments
Vicat Softening Point >= 80.0 °C
>= 176 °F
ASTM D 1525
Heat Distortion Temperature >= 75.0 °C
>= 167 °F
ASTM D 648
Flammability, UL94 V-0
V-0
Descriptive Properties Value Comments
Application General Purpose Profiles