Karina E 837-10/68-Y-CRA White PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 837-10/68-Y-CRA White PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.37 - 1.43 g/cc
1.37 - 1.43 g/cc
ASTM D 792
ASTM Color -1.39 - 0.21
-1.39 - 0.21
Color A, ME 12
1.67 - 3.27
1.67 - 3.27
Color B, ME 12
95.57 - 97.17
95.57 - 97.17
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore D 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Izod Impact, Notched >= 0.840 J/cm
>= 1.57 ft-lb/in
Method A; ASTM D 256
>= 28.4 J/cm
>= 53.2 ft-lb/in
Reversed Notch (Method E); ASTM D 256
Thermal Properties Metric English Comments
Vicat Softening Point >= 68.0 °C
>= 154 °F
ASTM D 1525
Heat Distortion Temperature >= 62.0 °C
>= 144 °F
ASTM D 648
Descriptive Properties Value Comments
Application General Purpose Injection Molded Parts
Torque 45
Nm; ME 37