Material Notes:
PVC compound with addition of nitrile rubber recommended for injection of boots, soles, and butcher shop bootsInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.18 - 1.22 g/cc
1.18 - 1.22 g/cc
NBR NM-IEC 60811-1-3
ASTM Color -1.90 - 1.1
-1.90 - 1.1
Color A, ME 12
2.8 - 5.8
2.8 - 5.8
Color B, ME 12
93.73 - 96.73
93.73 - 96.73
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 48 - 52

@Time 15.0 sec
48 - 52

@Time 0.00417 hour
ASTM D 2240