Material Notes:
Production Method: Made of atmospheric air by means of low temperature rectification. Application: Designed for use as protection media during welding, cutting and fusing of active and rare metals and their alloys, aluminum, and magnesium alloys, stainless chromium-nickel, heat-resistant alloys, and different grades of steel alloy, as well as for metals refining in metallurgy.Information Provided by Kazanorgsintez
Descriptive Properties Value Comments
Volume Content (%) 0.0005
Volume content of sum of carbonaceous compounds in conversion to CO2, Superior Quality
0.0007
Volume content of oxygen, Superior Quality
0.0009
Volume content of water steam that corresponds to max temperature of argon saturation of 61°C with water steam at pressure of 101.3 kPa, Superior Quality
0.001
Volume content of water steam that corresponds to max temperature of argon saturation of 58°C with water steam at pressure of 101.3 kPa, 1 Quality
0.001
Volume content of sum of carbonaceous compounds in conversion to CO2, 1 Quality
0.002
Volume content of oxygen, 1 Quality
0.005
Volume content of nitrogen, Superior Quality
0.01
Volume content of nitrogen, 1 Quality
99.987
Volume content of Argon, 1 Quality
99.993
Volume content of Argon, Superior Quality