Material Notes:
High flow, Air bag cover
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Moisture Absorption at Equilibrium 0.020 %
0.020 %
60% RH; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Shore D 54
54
ASTM D2240
Tensile Strength 29.0 MPa
4210 psi
ASTM D638
Elongation at Break 460 %
460 %
ASTM D638
Izod Impact, Notched NB
NB
ASTM D256
NB

@Temperature -40.0 °C
NB

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 HB
HB