Description: Kraton D1113 B is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 16%. It is supplied from South America in the physical form identified: D1113 BT - supplied as a dusted pelletRegion: South America, Europe, Asia Pacific, North America, and Japan Uses: Kraton D1113 B is used as an ingredient in formulating adhesives, sealants and coatings. It may also find use as a modifier of bitumen and polymers.Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Impact Modification; Footwear; and Bitumen ModificationPrimary antioxidant is a non-staining, phenolic antioxidant. The antioxidant package also contains a secondary antioxidant at the target level of 0.3%.Information provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 2781
Volatiles <= 0.50 %
<= 0.50 %
KM 04
Brookfield Viscosity 470 - 890 cP
470 - 890 cP
25% Toluene Solution at 25°C; KM 06
Melt Flow 24 g/10 min

@Load 5.00 kg,
Temperature 200 °C
24 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Ash 0.40 - 0.70 %
0.40 - 0.70 %
BT; ISO 247
Descriptive Properties Value Comments
Content Antioxidant
0.08-0.21%, KM 08
Polystyrene
15.1-17.3%, KM 03
Total Extractables
<1.0%, KM 05