LG Chemical B120 EPS, Non-Flame Retardant

Category Polymer , Thermoplastic , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer LG Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical B120 EPS, Non-Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Feature: Expendable Polystyrene, Non-Flame RetardantApplication: Package, Fruit/Fish Box, Floats, Pad, Ice BoxCAS No. 9003-53-6 and 109-66-0Information provided by LG Chemical
Physical Properties Metric English Comments
Water Absorption 0.24 %
0.24 %
[g/100cm<sup>2</sup>], 30g/L; KS M 3808
0.25 %
0.25 %
[g/100cm<sup>2</sup>], 25g/L; KS M 3808
0.30 %
0.30 %
[g/100cm<sup>2</sup>], 15g/L; KS M 3808
0.30 %
0.30 %
[g/100cm<sup>2</sup>], 20g/L; KS M 3808
Mechanical Properties Metric English Comments
Flexural Yield Strength 0.161 MPa
23.3 psi
15g/L; KS M 3808
0.294 MPa
42.7 psi
20g/L; KS M 3808
0.382 MPa
55.5 psi
25g/L; KS M 3808
0.441 MPa
64.0 psi
30g/L; KS M 3808
Impact 0.92
0.92
[kg/cm<sup>2<sup>], 15g/L; KS M 3808
1.32
1.32
[kg/cm<sup>2<sup>], 20g/L; KS M 3808
1.85
1.85
[kg/cm<sup>2<sup>], 25g/L; KS M 3808
2.4
2.4
[kg/cm<sup>2<sup>], 30g/L; KS M 3808
Thermal Properties Metric English Comments
Thermal Conductivity 0.0337 W/m-K
0.234 BTU-in/hr-ft²-°F
30g/L; KS M 3808
0.0349 W/m-K
0.242 BTU-in/hr-ft²-°F
25g/L; KS M 3808
0.0372 W/m-K
0.258 BTU-in/hr-ft²-°F
20g/L; KS M 3808
0.0395 W/m-K
0.274 BTU-in/hr-ft²-°F
15g/L; KS M 3808