Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LG Chemical B240 EPS, Non-Flame Retardant

Category Polymer , Thermoplastic , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer LG Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical B240 EPS, Non-Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Feature: Expendable Polystyrene, Non-Flame RetardantApplication: Package, Fruit/Fish Box, Floats, Pad, Ice BoxCAS No. 9003-53-6 and 109-66-0Information provided by LG Chemical
Physical Properties Metric English Comments
Water Absorption 0.45 %
0.45 %
[g/100cm<sup>2</sup>], 30g/L; KS M 3808
0.50 %
0.50 %
[g/100cm<sup>2</sup>], 25g/L; KS M 3808
0.75 %
0.75 %
[g/100cm<sup>2</sup>], 20g/L; KS M 3808
0.83 %
0.83 %
[g/100cm<sup>2</sup>], 15g/L; KS M 3808
Mechanical Properties Metric English Comments
Flexural Yield Strength 0.186 MPa
27.0 psi
15g/L; KS M 3808
0.255 MPa
37.0 psi
20g/L; KS M 3808
0.333 MPa
48.4 psi
25g/L; KS M 3808
0.412 MPa
59.7 psi
30g/L; KS M 3808
Impact 0.85
0.85
[kg/cm<sup>2<sup>], 15g/L; KS M 3808
1.3
1.3
[kg/cm<sup>2<sup>], 20g/L; KS M 3808
1.7
1.7
[kg/cm<sup>2<sup>], 25g/L; KS M 3808
2.1
2.1
[kg/cm<sup>2<sup>], 30g/L; KS M 3808
Thermal Properties Metric English Comments
Thermal Conductivity 0.0349 W/m-K
0.242 BTU-in/hr-ft²-°F
30g/L; KS M 3808
0.0360 W/m-K
0.250 BTU-in/hr-ft²-°F
25g/L; KS M 3808
0.0372 W/m-K
0.258 BTU-in/hr-ft²-°F
20g/L; KS M 3808
0.0407 W/m-K
0.282 BTU-in/hr-ft²-°F
15g/L; KS M 3808
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved