Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LG Chemical LGflex GL300 Plasticizer

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer LG Chemical
Trade Name LGflex
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical LGflex GL300 Plasticizer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Excellent Viscosity, Heat Stability and Non-endocrine disrupterApplication: PVC Calenderings/Leathers, Sheets, Gloves, HoseInformation provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 0.981 - 0.987 g/cc
0.981 - 0.987 g/cc
Volatiles 3.8 %

@Time 3600 sec
3.8 %

@Time 1.00 hour
Loss
7.2 %

@Time 7200 sec
7.2 %

@Time 2.00 hour
Loss
Viscosity 82 cP
82 cP
Molecular Weight 390.56 g/mol
390.56 g/mol
Mechanical Properties Metric English Comments
Tensile Strength at Break 22.6 MPa
3280 psi
Elongation at Break 405 %
405 %
50% Modulus 0.00618 GPa
0.896 ksi
100% Modulus 0.0102 GPa
1.48 ksi
Thermal Properties Metric English Comments
Melting Point -48.0 °C
-54.4 °F
Freezing Point
Boiling Point 400 °C
752 °F
Flash Point 238 °C
460 °F
Optical Properties Metric English Comments
Refractive Index 1.484 - 1.49
1.484 - 1.49
Electrical Properties Metric English Comments
Volume Resistivity >= 2.00e+11 ohm-cm
>= 2.00e+11 ohm-cm
Chemical Properties Metric English Comments
Acid Value <= 0.020
<= 0.020
KOH mg/g
<= 0.070
<= 0.070
After Heating, KOH mg/g
Descriptive Properties Value Comments
Color <20 APHA
Ester Value 284-290
Flexible Temperature -8 kg/cm2
G=3.17x10<sup>3<sup>
Heat Loss <0.07%
Users viewing this material also viewed the following: