Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LG Chemical SBR 1500 High Acrylonitrile Polymer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer LG Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical SBR 1500 High Acrylonitrile Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: NSBR 1500 is a cold polymerized styrene-butadiene copolymer with staining stabilizer. The cold polymerized SBR exhibits better abrasion, higher tensile strength and higher modulus than the hot polymerized SBR. SBR 1500 has more tack than other SBR due to the rosin acid emulsifying system in polymerization. This characteristic provides easier processing properties and better cohesion between rubber to rubber interface. However, due to the staining stabilizer, it can be used only in applications where color is of secondary importance.Applications: SB 1500 can be used to tire, camelback, molded and extruded industrial goods and dark colored products where staining and color are not limiting factors.CAS No: 9003-55-8Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
Volatiles 0.30 %
0.30 %
Mooney Viscosity 52

@Temperature 100 °C
52

@Temperature 212 °F
ML 1+4
Ash 0.20 %
0.20 %
Mechanical Properties Metric English Comments
Tensile Strength at Break 28.4 MPa

@Temperature 145 °C,
Time 2100 sec
4120 psi

@Temperature 293 °F,
Time 0.583 hour
ASTM D412
Elongation at Break 520 %

@Temperature 145 °C,
Time 2100 sec
520 %

@Temperature 293 °F,
Time 0.583 hour
ASTM D412
300% Modulus 0.0157 GPa

@Temperature 145 °C,
Time 2100 sec
2.28 ksi

@Temperature 293 °F,
Time 0.583 hour
ASTM D412
Chemical Properties Metric English Comments
Styrene Content 23.5 %
23.5 %
Bound
Descriptive Properties Value Comments
Color Dark brown Bale
Components HAF
50, ASTM D3185
SBR 1500
100, ASTM D3185
Stearic Acid
1, ASTM D3185
Sulfur
1.75, ASTM D3185
TBBS
1, ASTM D3185
ZnO
3, ASTM D3185
Organic Acid 0.061
Soap 0.001
Users viewing this material also viewed the following: