Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lehigh Technologies 200 Mesh Ground Reclaimed Whole Tire Rubber

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Lehigh Technologies, LLC
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehigh Technologies 200 Mesh Ground Reclaimed Whole Tire Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A free flowing black powder produced from vulcanized rubber materialInformation provided by Lehigh Technologies, LLC.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
Particle Mesh Size 140 Mesh
140 Mesh
0
170 Mesh
170 Mesh
0
200 Mesh
200 Mesh
0-10 %
Carbon Black Loading 26 - 38 %
26 - 38 %
Ash 8.0 - 12 %
8.0 - 12 %
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
Descriptive Properties Value Comments
Acetone Extractables wt.% 8.0 - 22.0
Fiber Content Max wt.% 0.5
Loss on Heating 1
Metal Content Max wt.% 0.1
Natural Rubber wt.% 10.0 - 36.0
Rubber Hydrocarbon Content 42.0 - 47.0