Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lehmann & Voss LUVOCOM® 1-8501 Polyamide 66, with glass fiber, lubricant modified, heat stabilized

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Fiber/PTFE Filled
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 1-8501 Polyamide 66, with glass fiber, lubricant modified, heat stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.dynamic stressBearings, sleeves, sliding elements, control disks, gear wheels, duty parts in switches.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.42 g/cc
1.42 g/cc
ISO 1183
Water Absorption <= 1.0 %
<= 1.0 %
23°C/24h
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
Mechanical Properties Metric English Comments
Tensile Stress 175 MPa
25400 psi
Elongation at Yield 2.5 %
2.5 %
3.3 %
3.3 %
flexural
Modulus of Elasticity 10.0 GPa
1450 ksi
Flexural Strength 240 MPa
34800 psi
Flexural Modulus 8.50 GPa
1230 ksi
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
edgewise; ISO 179 1eU
4.00 J/cm²

@Temperature -30.0 °C
19.0 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
ISO 179 1eA
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 110 °C
230 °F
160 °C
320 °F
short term
Electrical Properties Metric English Comments
Surface Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Insulation Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Processing Properties Metric English Comments
Processing Temperature 290 °C
554 °F
mass temp
Nozzle Temperature 280 - 300 °C
536 - 572 °F
Zone 1 290 - 310 °C
554 - 590 °F
Zone 2 290 - 310 °C
554 - 590 °F
Zone 3 290 - 310 °C
554 - 590 °F
Mold Temperature 90.0 - 120 °C
194 - 248 °F
Drying Temperature 75.0 °C

@Time 21600 - 57600 sec
167 °F

@Time 6.00 - 16.0 hour
Dehumidifying dryer
105 °C

@Time 14400 - 21600 sec
221 °F

@Time 4.00 - 6.00 hour
Vacuum Dryer
Descriptive Properties Value Comments
Color natural color (grey)
Users viewing this material also viewed the following: