Material Notes:
Information provided by Loxim Industries
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
ASTM D792
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D1299
Mechanical Properties Metric English Comments
Tensile Strength at Break 180 MPa
26100 psi
ASTM D683
Elongation at Break 3.0 - 4.0 %
3.0 - 4.0 %
ASTM D638
Flexural Modulus 8.50 GPa
1230 ksi
ASTM D790
Izod Impact, Notched 1.10 J/cm
2.06 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 250 °C
482 °F
ASTM D1525, HDT Method B
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Users viewing this material also viewed the following: