Material Notes:
These popular lithium type greases are excellent for a wide range of lubrication demands thus reducing the need to carry large grease inventories. They show exceptional resistance to water, steam, and other adverse conditions. Available in 4 NLGI densities for a variety of applications. Applications: Multi-purpose, general greasing, bearings.630 Series Greases are available in Cartridges, Tubes, Cans, Pails, 1/4 Drums & Drums.Information provided by Lubriplate
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 750 SUS
750 SUS
Kinematic Viscosity at 40°C (104°F) 135 cSt
135 cSt
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 265
265
Unknown Amount of Work
Penetration P(60), 1/10 mm 295
295
Unknown Amount of Work
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -17.8 °C
0.000 °F
Approx. Cold test
Dropping Point 193 °C
380 °F
ASTM Test
Descriptive Properties Value Comments
Antiwear (AW)/ Extreme Pressure (EP) AW/EP
NLGI Grade 2
Rust/Oxidative Additives YES
Water Resistant YES