Lubriplate FMO 900 AW USP Mineral Oil-Based Food Machinery Grade Oil

Category Fluid , Lubricant , White Mineral Oil (WMO)
Manufacturer Lubriplate Lubricants
Trade Name FMO
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubriplate FMO 900 AW USP Mineral Oil-Based Food Machinery Grade Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
For use where a Class H-1 oil is required. Manufactured in nine ISO grades for a variety of applications. Anti-wear fortified. NOTE: FMO-350AW is also available in a red and orange color which helps in leak detection. FMO-1100AW and FMO-2400AW pass 12 stages of the FZG test. The original FMO Series products without the anti wear additive system are still available.FMO Series Oils are available in Bottles, Jugs, Pails, 1/4 Drums & Drums.H-1 Class Lubricants are manufactured with ingredients that comply with FDA regulation 21 CFR 178.3570 for lubricants with incidental contact with the edible product.Information provided by Lubriplate
Physical Properties Metric English Comments
Viscosity Measurement 99
99
Viscosity Index
150
150
ISO Grade
Saybolt Viscosity at 100°F 856 SUS
856 SUS
Saybolt Viscosity at 210°F 83 SUS
83 SUS
Kinematic Viscosity at 40°C (104°F) 160 cSt
160 cSt
Kinematic Viscosity at 100°C (212°F) 15 cSt
15 cSt
Thermal Properties Metric English Comments
Pour Point -17.8 °C
0.000 °F
Flammability Test 540
540
[°F] Fire Point
Flash Point 232 °C
450 °F
Descriptive Properties Value Comments
SAE Gear Oil No. 90
SAE No. 40