Lubriplate MV-HO Petroleum-Based Heavy-Duty Hydraulic Oil

Category Fluid , Lubricant
Manufacturer Lubriplate Lubricants
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubriplate MV-HO Petroleum-Based Heavy-Duty Hydraulic Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ISO 32 petroleum-based oil for low temperature applications. Low Temp Hydraulic Oils are available in Jugs, Pails, 1/4 Drums & Drums.Information provided by Lubriplate
Physical Properties Metric English Comments
Viscosity Measurement 32
32
ISO Grade
199
199
Viscosity Index
Saybolt Viscosity at 100°F 186 SUS
186 SUS
Saybolt Viscosity at 210°F 53 SUS
53 SUS
Kinematic Viscosity at 40°C (104°F) 35 cSt
35 cSt
Kinematic Viscosity at 100°C (212°F) 8.0 cSt
8.0 cSt
Thermal Properties Metric English Comments
Pour Point -45.6 °C
-50.0 °F
Flammability Test 380
380
[°F] Fire Point
Flash Point 177 °C
350 °F
Descriptive Properties Value Comments
SAE Gear Oil No. 75
SAE No. 5W-20