Lubriplate SYN LUBE 320 PAO-Based Multi-Purpose Synthetic Fluid

Category Fluid , Lubricant , Polyalphaolefin (PAO)
Manufacturer Lubriplate Lubricants
Trade Name SYN LUBE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubriplate SYN LUBE 320 PAO-Based Multi-Purpose Synthetic Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PAO-based zinc free fluids formulated with state of the art additives to provide outstanding performance over extended drain intervals.Applications: Syn-Lube 150, 220, 320, 460 & 680 are recommended for many types of rotary screw and piston type air compressors, hydraulic systems, blowers, and turbine oil applications. Available in Jugs, Pails, 1/4 Drums and DrumsInformation provided by Lubriplate
Physical Properties Metric English Comments
Viscosity Measurement 157
157
Viscosity Index
320
320
ISO Grade
Saybolt Viscosity at 100°F 1545 SUS
1545 SUS
Kinematic Viscosity at 40°C (104°F) 310 cSt
310 cSt
Kinematic Viscosity at 100°C (212°F) 35 cSt
35 cSt
Thermal Properties Metric English Comments
Pour Point -45.6 °C
-50.0 °F
Flammability Test 585
585
[°F] Fire Point
Flash Point 282 °C
540 °F
Descriptive Properties Value Comments
SAE Gear Oil No. 80W-140
SAE No. 60