Lubriplate SYN SYN-1602 PAO-Based Multi-Purpose Grease

Category Fluid , Lubricant , Lithium Gellant , Polyalphaolefin (PAO)
Manufacturer Lubriplate Lubricants
Trade Name SYN
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubriplate SYN SYN-1602 PAO-Based Multi-Purpose Grease.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Manufactured with 100% PAO base fluids and thickened with lithium complex for superior oxidation stability, better wear protection, and significantly better operating temperature ranges. Fortified with additives to prevent rust and corrosion, as well as reduce grease bleed. Applications: Multi-purpose, heavy-duty applications. SYN-1600 Series Greases are available in Pails, 1/4 Drums & Drums. SYN-1601 & SYN-1602 are also available in Cartridges. Information provided by Lubriplate
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 2066 SUS
2066 SUS
Kinematic Viscosity at 40°C (104°F) 446 cSt
446 cSt
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 265
265
Unknown Amount of Work
Penetration P(60), 1/10 mm 295
295
Unknown Amount of Work
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -42.8 °C
-45.0 °F
Approx. Cold test
Dropping Point 260 °C
500 °F
ASTM Test
Descriptive Properties Value Comments
Antiwear (AW)/ Extreme Pressure (EP) AW/EP
NLGI Grade 2
Rust/Oxidative Additives YES
Water Resistant YES