Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol ESTANE® 5714 Ether Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® 5714 Ether Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Low Temperature Flexibility, Excellent Abrasion, Fungal, and Chemical Resistance, and Hydrolytic Stability. Adhesives can be applied from solution or extruded as a melt coating. The resin is lightly dusted with calcium stearate and contains UV stabilizer.Uses: Various adhesive and fabric coating, magnetic media binder and cast films for laminationAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Noveon, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Viscosity 72000 cP

@Temperature 204 °C
72000 cP

@Temperature 399 °F
ASTM D-1084-88
Brookfield Viscosity 900 cP
900 cP
RVT Spindle #2, 20 RPM, 23°C, 15% T.S. in THF
3700 cP
3700 cP
RVT Spindle #2, 20 RPM, 23°C, 15% T.S. in Cyclohexanone
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ASTM D2240
Tensile Strength 31.0 MPa
4500 psi
ASTM D412/D638
Elongation at Break 530 %
530 %
ASTM D412/D638
100% Modulus 0.00480 GPa
0.696 ksi
ASTM D412/D638
300% Modulus 0.00900 GPa
1.31 ksi
ASTM D412/D638
Peel Strength 0.500 kN/m
2.85 pli
ASTM D-1876-72
1.50 kN/m
8.56 pli
ASTM D-1876-72
Thermal Properties Metric English Comments
Vicat Softening Point 71.1 °C
160 °F
ASTM D1525
Glass Transition Temp, Tg -38.0 °C
-36.4 °F
DSC
Ring & Ball Softening Point 174 °C
345 °F
ASTM E-28-92
Descriptive Properties Value Comments
Gradient Bar Tack Temperature 127°C
Open Time <5 sec