Lucite International Colacryl ® D60 Acrylic Dental Resin

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Lucite International
Trade Name Colacryl ®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Colacryl ® D60 Acrylic Dental Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A range of Methyl Methacrylate polymers designed for use as standard heat-curing denture base resins.Features: Fine free-flowing bead polymers containing residual peroxide initiator; Curing cycles from 2 hours using Colacryl® TS 1502 liquid; Designed to meet the requirements of ISO 1567/ADA 12; Choice of process properties including prolonged work time.Benefits: Cures water-white when processed with Colacryl® TS 1502 liquid; Reduced risk of micro-porosity in thicker sections; Improved colour stability when processed with Colacryl® TS1502.Information provided by Lucite International
Physical Properties Metric English Comments
Particle Size 60 - 80 µm
60 - 80 µm
Molecular Weight 900000 - 1.50e+6 g/mol
900000 - 1.50e+6 g/mol
Descriptive Properties Value Comments
Residual peroxide (%) .5 - .7
Work Time (min) 15