Material Notes:
Key Features: medium melt flow, medium modulus, UV-stabilized, polypropylene copolymer, high impact strength, excellent processabilityApplications: door and luggage compartment scruff plates, seat track covers, bezel trim, taillight access coversDescription: Astryn EPF30U medium melt flow, UV-stabilized, precolored polypropylene copolymer has excellent impact strength and processability. It was designed for a variety of automotive interior applications.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
ISO 2577
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 59
59
ISO 868
Tensile Strength, Yield 21.0 MPa
3050 psi
ISO R527
Elongation at Yield 7.0 %
7.0 %
ISO R527
Flexural Modulus 0.970 GPa
141 ksi
ISO 178
Izod Impact, Notched 22.0 J/cm

@Temperature 23.0 °C
41.2 ft-lb/in

@Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
50.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ISO 75