Material Notes:
Description: Hostacomâ„¢ BJ23A is a polypropylene copolymer that is used for appliance componentsFeatures: Good StiffnessGood FlowChemically CoupledGood Impact ResistanceInformation provided by Basell.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 78.6 MPa
11400 psi
ASTM D 638
Flexural Modulus 4.55 GPa
660 ksi
ASTM D790
Izod Impact, Notched 1.17 J/cm
2.20 ft-lb/in
73°F; ASTM D256
Izod Impact, Unnotched 6.41 J/cm
12.0 ft-lb/in
73°F; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 146 °C
295 °F
Unannealed; ASTM D648