Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

M Chemical GUARD DOGâ„¢ UV531 Light Absorber (Flake or Powder), Benzophenone Derivative

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer M Chemical Company, Inc.
Trade Name GUARD DOG™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M Chemical GUARD DOGâ„¢ UV531 Light Absorber (Flake or Powder), Benzophenone Derivative.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
GUARD DOG™ UV531(flake or powder) light stabilizer is a derivative of Benzophenone that has an exceptionally strong and broad-range of UV absorption properties (UV A 315 -400 nm and UV B 290 - 314 nm) throughout the UV spectrum. It is a highly efficient UV absorber and is recommended for thermoset plastics and coatings that function as ultraviolet screens for photosensitive substrates. It offers maximum polymer protection and low color contribution, retards yellowing and loss of physical properties. It is recommended for thick films (> 100 mm).Applications: Extremely effective in PE (film tape, injection and rotational molding, metallocene), PP (film, tape, fiber, injection molding), TPO, PVC (rigid and flexible), ABS resin, PU, Phenolic resin, Paraffin, Rubber.Performance Benefits:Strong and broad UV absorption with low color contribution and no loss during processingPerformance synergy with HALS. Does not migrate to the surface.Excellent compatibility with polymers and other stabilizer chemistries, especially with polyolefins.Typical Properties:Free flowing powder and flakeSolubility (g/100g @ 25°C): Acetone 74.3, Benzene 72.7, Ethyl Acetate 180, MEK 65, Toluene 70
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc

@Temperature 20.0 °C
1.16 g/cc

@Temperature 68.0 °F
Particle Size <= 0.329 µm
<= 0.329 µm
Molecular Weight 326.43 g/mol
326.43 g/mol
Absorption Coefficient <= 31.7
<= 31.7
10 mg UV/l of Toluene
Thermal Properties Metric English Comments
Melting Point 47.0 - 49.0 °C
117 - 120 °F
Descriptive Properties Value Comments
CAS Number 1843-05-6
Molecular Formula C21H26O3
Name 2-hydroxy-4-n-octooxybenzophenone