Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

MRC Polymers MAXTELâ„¢ 650-BK Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer MRC Polymers
Trade Name MAXTEL™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MRC Polymers MAXTELâ„¢ 650-BK Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
• For injection molding• Excellent process ability with high flow.Information provided by MRC Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ISO 1183
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Ash 1.1 %
1.1 %
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength 28.0 MPa
4060 psi
ISO 527
Elongation at Break 13 %
13 %
ISO 527
Flexural Strength 28.0 MPa
4060 psi
ISO 178
Flexural Modulus 1.20 GPa
174 ksi
ISO 178
Izod Impact, Notched (ISO) 2.90 kJ/m²
1.38 ft-lb/in²
ISO 180
Users viewing this material also viewed the following: